Study on the Deterioration of Ultra High Performance Concrete under the Coupling of Wet and Dry Cycling and Sulfate Erosion

Xuetao Xia *

School of Civil Engineering and Communication, North China University of Water Resources and Electric Power, Zhengzhou, 450045, China.

*Author to whom correspondence should be addressed.


Abstract

Ultra-high-performance concrete (UHPC) is exposed to combined sulfate attack and wet–dry cycling in saline soil and coastal environments, and its deterioration is more complex than under simple immersion. To examine the evolution of UHPC performance under these coupled conditions, specimens were assigned to a water control group (S0) and a 5 wt% Na₂SO₄ solution group (S5) and subjected to six wet–dry cycles. Each cycle comprised 7 days of immersion and 8 days of drying at 80 °C. Mass loss rate, relative dynamic modulus of elasticity (RDEM), compressive strength and flexural strength were assessed. The results showed an overall two-stage pattern of initial densification and strengthening followed by damage and deterioration. Mass loss rates were initially negative because of continued hydration and water absorption, before gradually increasing. The S5 group changed from negative to positive values earlier than S0; after the sixth cycle, mass loss rates were 0.60% for S0 and 0.80% for S5. RDEM peaked after the second cycle and then decreased to approximately 0.93 and 0.87 for S0 and S5, respectively, corresponding to reductions of approximately 7% and 13%. Relative compressive strength also increased before decreasing to approximately 0.98 and 0.94, corresponding to reductions of approximately 2% and 6%. Peak flexural loads declined after the second cycle; after six cycles, these were approximately 5.1 kN and 4.3 kN for S0 and S5, respectively, with lower residual load-bearing capacity in the later stages for S5. Overall, coupled sulfate exposure and wet–dry cycling were associated with more pronounced deterioration of UHPC, consistent with the development of internal microcracks and weakening of the steel fibre–matrix interface. These findings provide experimental evidence relevant to durability evaluation of UHPC in saline soil and coastal environments.

Keywords: Ultra-high-performance concrete, sulfate attack, wet–dry cycling, mass loss rate, relative dynamic modulus, compressive strength, flexural strength


How to Cite

Xia, Xuetao. 2026. “Study on the Deterioration of Ultra High Performance Concrete under the Coupling of Wet and Dry Cycling and Sulfate Erosion”. Advances in Research 27 (6):404-11. https://doi.org/10.9734/air/2026/v27i61783.

Downloads

Download data is not yet available.